🕑 Reading time: one minute

Repair of small-scale, medium and large cracks in concrete and repair of crushed concrete is required to heighten the strength and durability of damaged concrete members.

Repair of small and medium cracks in concrete

Small-scale and medium cracks in reinforced physical and masonry structures reduce their strength considerably to bear the design loads. Thus repair of such cracks is necessary to restore the designed strength of members. The repair of small and medium cracks is done past first marking out the disquisitional damaged zones in concrete members. And then these cracks can exist repaired by injecting cement grout or chemical grouts or by providing jacketing. The smaller cracks less than 0.75 mm width can be effectively repair by using pressure level injection of epoxy. The surface of the fellow member virtually cracks is thoroughly cleaned. Loose materials are removed and plastic injection ports are placed along the length of crack at an interval equal to the thickness of the structural member. These ports are placed on both sides of the member and secured in placed with the help of epoxy seal. When the epoxy seal has hardened, the low viscosity resin is injected into one port at a time starting from the port at lowest level and moving upwards. The injection through port is continued till the resin flows out from the adjacent port or from the other side of the fellow member. Then the current injection port is closed and epoxy injection is connected from the next port.

Injection grouting for concrete crack repair

This procedure is carried out in sequence till all the ports and cracks are filled with the grout. This method can be used for all types of structural members such are beams, columns, walls and slabs. This method tin can also to repair of small cracks in private masonry blocks or for filling large continuous cracks.

Repair of Big Cracks and Crushed Concrete:

Repair of large cracks (cracks wider than 5mm) and crushed physical and masonry structure cannot be washed using force per unit area injection or grouting. For repair of big cracks and crushed physical, following procedure can exist adopted: 1. The surface of cracks or crushed concrete is cleaned and all the loose materials are removed. These are then filled with quick setting cement mortar grouts. 2. If the cracks are big, then these cracks are dressed to have a 5 groove at both sides of the fellow member for easy placement of grouts.

Repair of large cracks in concrete and masonry walls

Fig: Filling of cement mortar and stone chips in large cracks in masonry walls.

3. For cracks which are very large, filler materials such as stone chips can be used. four. Boosted reinforcement and shear reinforcements can be used for heavily damaged concrete members or wherever necessary based on requirements. These additional reinforcement should exist protected from corrosion by using polymer mortar or epoxy coatings. 5. For damaged walls and roofs, additional reinforcement in the form of mesh is used on one side or both sides of the members. These mesh should sufficiently tied with existing members.

Reinforcement meshes in repair of roof slabs and walls

Fig: Reinforcement meshes in repair of roof slabs and walls. ane. Wire mesh on forepart face, 2. Clamps, three. Wire mesh on dorsum face, iv. Cement plaster, 5. Crack in member.

6. Stitching of cracks are done to foreclose the widening of the existing cracks. In this case, holes of 6 to 10mm are drilled on both sides of the crack. Then these drilled holes are cleaned, legs of stitching dogs are anchored with short legs. The stitching of cracks is not a method of crack repair or to gain the lost strength, this method is used to prevent the cracks from propagating and widening.